This is Enta.

We've started to see some changes in the crack test results.

22 days old

No. 1 Plastic Spacer, 22nd

The No. 1 plastic spacer remains the same.

No. 2 PC Spacer, the 22nd

The PC spacers are the same as before.

No. 3: Las Only, 22nd

Changes have begun to appear in the test specimens made ofラス alone.

The test specimens themselves are placed side by side in the same position.

So the conditions are the same.

Crack Location (Lath Only)

There's a small crack here.

Last Show: "Crack" on the 22nd

It's faint.

I think the changes are probably due to factors like temperature and sunlight.

I wonder if last week's rain had something to do with it...

I hope things keep changing for the better like this lol

 

It would probably be funnier for the sake of the joke if at least one of them were completely shattered, but in reality, it’s probably pretty dull.

And I have a feeling that, in the end, they'll take a photo of it from directly above, draw a line along the crack to measure its length, and make a close call on the verdict lol

Well, I guess that's just how it goes, huh? lol

Like, how cracks form and stuff.

 

The test specimens are located in Azumino City, Nagano Prefecture, where there’s a huge temperature difference between summer and winter, so I’m hoping for at least a little improvement.

If we keep ramping up the intensity like this as we head into summer, I think we'll start to see some changes.

 

This crack test is surprisingly low-key, but please bear with me lol

By the way, I plan to keep an eye on this for at least a year or so.

 